Fil fil fil mono fil konsiste de yon sèl fil asye galvanised ak kat -pwen fil trese nan entèval regilye. Li konfòm ak estanda ASTM A641 (ba-kabòn) oswa ASTM A121 (segondè -tansyon). Aplikasyon komen yo gen ladan fwontyè fèm, medyàn gran wout, ak perimèt sekirite kote yon baryè ki pi lejè men efikas.
Espesifikasyon teknik
|
Dyamèt fil (nwayo) |
2.0 mm, 2.5 mm, oswa 2.8 mm (± 0.05 mm) |
|
Barb espas |
100 mm (4″) oswa 125 mm (5″), espas koutim ki disponib jiska 75 mm |
|
Longè barb |
1.5 mm a 2.0 mm soti nan sifas nwayo |
|
Fòs kraze (ba-kabòn) |
350-500 MPa pou chak ASTM A641 |
|
Fòs kraze (wo rupture) |
1100-1400 MPa pa ASTM A121 |
|
Zenk kouch pwa |
plonje cho 220 g/m² (minimòm) oswa elektwogalvanize 12-25 g/m² |
|
Anbalaj |
50 m, 100 m, oswa 200 m bobin sou bobin an bwa oswa bobin plastik |



Materyèl Klas & Chimi
Fil asye ki ba-kabòn
(SAE 1006 oswa 1008)
C mwens pase oswa egal a 0.08%, Mn 0.30–0.50%, P mwens pase oswa egal a 0.030%, S mwens pase oswa egal a 0.035%
Fil asye wo-tansyon
(SAE 1070)
C 0.65-0.75%, Mn 0.60-0.90%, Si 0.15-0.30%
PVC kouch
(si aplike)
epesè 0.4-0.6 mm, konfòme ak RoHS, UV estabilize pou 5+ ane
FAQ
Q1: Ki sa ki longè maksimòm woulo liv san yon épissure?
Pou fil 2.0 mm, nou ka pwodwi jiska 500 m longè kontinyèl san okenn épissure. Pou 2.8 mm, maksimòm se 300 m.
Q2: Èske ou ofri en fe mono strand fil fè?
Wi, ak klas 304 oswa 316. Pwosesis barbing la se menm bagay la, men fòs la rupture se alantou 700-800 MPa.
Q3: Konbyen tan cho-dip galvanised mono strand dire nan yon anviwònman maren?
Tipikman 10-15 ane. Pou plis lavi, ajoute yon kouch PVC oswa itilize 316 Nerjaveèi.
Baj popilè: mono strand fil fè fil, Lachin mono strand fil fè manifaktirè, Swèd, faktori